ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Influence of Quickened Lime on Slag-Forming Rate
Hao Huaqiang, Cui Penghui, Jiang Wufeng, Hao Suju , Zhang Yuzhu
Special Steel . 2016, (4): 1 -4 .