Establishment of FeO Thickness Percentage Model of High Carbon Steel Coil at Cooling Line and Its Application
Wang Yu , Cheng Xiaoru , Fan Jingguo , Shen Jinlong
Special Steel . 2016, (2): 8 -11 .