ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Experiment on Primary Recrystallization Annealing Process of 0.42 % Cu Hi-B Steel Manufactured by Simulated CSP Flowsheet
Ma Li , Zhao Gang , Huang Rusheng , Liu Zhanlong , Ye Fan , Tang Shunqi
Special Steel . 2016, (2): 66 -69 .