Controlled Rolling Process of Hot Rolled Tube Bloom of CB890QL Steel for Crawler Crane
XUAN Kangle, JIANG Hongliang, ZHANG Xinwen, SUN Zhiwei, ZHANG Chunxiang, GAO Huayao
Special Steel . 2022, (4): 36 -40 .