Control of Dynamic Secondary Cooling Process for Vertical-Bending 220 mm x 220 mm Casting Bloom of Austenite Stainless Steel
Du Chenwei, Li Yujun, Zhang Jiaquan, Tian Guanqing, Lii Longting, Zheng Xinguo , Li Jingyu
Special Steel . 2015, (6): 26 -29 .