Numerical Simulation of Transferring Characteristics of Liquid Steel in Mould for Continuous Casting H-Beam Bloom
Ruan Fei , Feng Kongfang , Ma Jie , Bai Liang , Wang Bo , Zhang Jieyu
Special Steel . 2015, (5): 5 -8 .