Effect of Forging and Conditioning Heat Treatment on Grain Size of Super-High Strength Steel 23Co-Ni
Wang Rui , Gong Wei, Jiang Zhouhua , Xue Xiangxin
Special Steel . 2015, (6): 39 -41 .