Effect of Cold Reduction Ratio on Primary Recrystallization Texture of Hi-B High Magnetic Induction Oriented Silicon Steel
Zhu Weijie, Zhao Gang, Wang Chang, Huang Jie , Du Liang
Special Steel . 2015, (6): 53 -55 .