Effect of Fluorite Content on Physical Properties of Mould Powder and Mineralogical Structure of Flux Film
Wang Kaiqiang, Han Xiuli, Liu Lina, Ding Ning, Zhang Yifei
Special Steel . 2016, (1): 9 -12 .