Dynamic Recrystallization of 0.03Nb-0.15Ti Microalloying Low-Carbon High-Strength Steel
Gan Xiaolong , Han Bin , Wang Shuize , Cai Zhen , Zhu Wanjun
Special Steel . 2015, (5): 51 -54 .