Effect of Shaping and Surface Treatment Process on Release Rate of Nickel in Stainless Steel 316L
Yuan Junping , Wu Haichao , Lu Huanxun , Chen Shaoxing , Bo Hairui , Huang Yuheng
Special Steel . 2015, (5): 59 -63 .