Cold-Work Hardening and Wear-Corrosion Resistance of Silver-Containing High-Nitrogen Nickel-Free Antibacterial Stainless Steel HNSAg
Yuan Junping, Wang Chang, Chen Shaoxing, Lu Huanxun, Shen Keya , Huang Yuheng
Special Steel . 2015, (6): 59 -62 .