Cause for Submerged Entry Nozzle Blocking during Casting of Aluminium Killed Steel SPHC and Control Process
Zhang Dajiang, Wang Cuina, Xiang Hua, Wan Guoxi , Zheng Fei
Special Steel . 2015, (3): 30 -33 .