Model of Austenite Grain Growth during a Continuous Heating Process of Steel 42CrMo for Bearing Ring of Shield Tunneling Machine
Zheng Yu, Jiang Peiyang , Zhang Haozhen, Zhou Leyu, Zhang Chaolei, Liu Yazheng
Special Steel . 2014, (6): 57 -59 .