Development and Production of 4Cr5Mo2V Large Die Steel  640 mm x 1100 mm Forged Bloom for Automobile Die Casting
ZHOU Xu, WANG Shijun, YAN Lei, DENG Li, ZHANG Yongqiang
Special Steel . 2022, (4): 70 -74 .