ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Numerical Simulation on Temperature Change of 325 mm x 280 mm Bloom of Bearing Steel during Casting-Breakdown Process Flowsheet
Dang Aiguo , Cui Juan , Li Yongchao , Feng Yan
Special Steel . 2015, (2): 17 -20 .