Finite Element Simulation on Wearing of Roll for Rough Mill of Hot Continuous Rolling Mill and Process Optimization
Li Xiaolong , Zhou Lixin , Zhou Dunshi , Feng Liang
Special Steel . 2015, (2): 21 -24 .