ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Optimization on Remelting Process of 1.1 t ESR Ingot of Blade Steel 1Cr12Ni2Mo2VN
Yan Qingzhong , Chen Lie , Li Fawen , Zuo Hui , Wu Bin , Lu Yanming , Li Zheng , Zhao Haidong , Cheng Guoguang
Special Steel . 2015, (2): 44 -47 .