ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Cooling Rate on Inclusions and Structure of 0.45C Steel Casting Billet
Zhang Qingjun , Wu Yaoguang , Cui Zhimin , Zhu Liguang
Special Steel . 2015, (2): 48 -51 .