Gear Steel 40CrMo Surface Laser Cladding 0.60C-15.25Cr-l. 85Mo Powder process and Its Structure and Properties
Chen lei, Xia Zhixin, Jia Shuai, Zhao Jing, Fu Geyan, Shi Shihong
Special Steel . 2016, (1): 22 -24 .