Practice of Process for Production of Weathering Steel S355J2 by 70 t LD-LF-VD-CC Flowsheet
Li Xuezhao, Li Shuangjiang, Dong Lixia, Bai Xiaofeng
Special Steel . 2016, (1): 37 -39 .