ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Optimization and Development of 500 MPa Ti-Nb Microalloy High Strength Steel for Auto
Yin Sheng, Zhu Hongdan
Special Steel . 2016, (1): 68 -70 .