Effect of Carbon and Boron Content on Mechanical Properties of Casting Bloom of Low Carbon Cold Heading Steel at Elevated Temperature
Duan Luzhao, Su Yuhui, Cui Juan, Li Yongchao , Liu Chao
Special Steel . 2015, (4): 63 -65 .