A Study on Optimization of a 20 t Tundish Structure for 3-Strands Casting Based on Hydraulic Simulated Test
Yang Lingzhi, Zhu Rong, Li Chao, Lin Tengchang, Wu Bing, Liang Jianguo
Special Steel . 2015, (1): 1 -4 .