Heat Treatment, Structure and Properties of High-Strength-Toughness Steel 12Cr2Mo 406 mm x 40.5 nun Tube for High Pressure Boiler
Zhang Zhicheng , Li Yongdeng , Ruan Linghui, Wu Kaiming
Special Steel . 2015, (1): 52 -55 .