Structure and Properties of (30 ~ 90) mm x (400 ~ 605) mm Cold-Working Die Flat Steel Cr12Mo1V1 (D2)
Liu Zhentian, Chi Hongxiao, Ma Dangshen, Kang Aijun, Zhou Jian
Special Steel . 2015, (1): 65 -68 .