Numerical and Physical Simulation for Effect of Baffle Structure on Flow Characteristics of Liquid in a 46 t Tundish
Li Yang , Jin Yan , Feng Xuewu , Chang Zhengsheng , Jin Yeilei
Special Steel . 2014, (5): 15 -18 .