Process Practice of Rod Coil of High Carbon Stainless Steel 9Cr18 Produced by 50 t EAF-AOD-LF-VD-CC-Rolling Flow Sheet
Li Zhongzhi , Yang Qingmin , Yu Yajie , Yu Quangong , Nie Xianfei , Zhou Yiling
Special Steel . 2014, (5): 37 -39 .