Development of 600 MPa Low Silicon and Nb-Ti Microalloying High Quality 3.5 mm Hot-Rolled Dual Phase Steel Plate
Yin Sheng , Cai Xiaohui , Zhu Hongdan
Special Steel . 2014, (5): 47 -49 .