Reversible Precipitation Reaction between M(CN) and M 23( CN) 6 in Heat Resistant Steel 5Cr21Mn9Ni4Nb2WN
He Yanxu , Liu Xuesheng , Ding Lei
Special Steel . 2014, (5): 61 -63 .