ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Application of Vibrating-Exciting Nucleation Technology in 45 t Q345B Steel Ingot Casting
Wang Chao', Zhang Hui, Wang Minglin'', Ma Zhongwei, Zhao Pei
Special Steel . 2014, (4): 20 -23 .