Pilot Production of High Strength Low Alloy Steel Q345B Supper-Heavy Plate by Compound-Rolling Process
Chen Zhenye, Zhang Xiaoli, Zhang Yunfei, Yang Yuehui, Wei Ming , Li Hongwen
Special Steel . 2014, (4): 31 -33 .