An Analysis on Crane- Conveying Fracture of Partial 170 mm Casting Slab of Steel 25SiMn2 and Improving Measures
Su Chunxia, Chen Benwen, Fu Chao, Sun Diandong , Wang Yong
Special Steel . 2014, (4): 34 -35 .