Effect of Finish Rolling and Wire Coiling Temperature on Structure Texture and Properties of 72A Tire Cord Steel Coil
Liao Shulun, Lu Lihua, Shen Kui , Ma Han
Special Steel . 2014, (4): 59 -61 .