ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

A Study on Mold Powder for High Aluminium Austenite Non-Magnetic Steel 20Mn23Al2V Slab Casting
Zhang Yubin, Wen Guanghua, Yu Xiong, Tang Ping
Special Steel . 2013, (6): 22 -25 .