Effect of Prestrain on Bake Hardening property of Ultra-Low Carbon Bake Hardening (ULC-BH) Steel
Yang Xi , Li Weijuan, Jin Xiaolong, Sun Chengqian
Special Steel . 2014, (1): 61 -64 .