Commercial Pilot Production of Vanadium Steel SG45 by V 2O 5 Self-Reducing Direct Alloying in Ladle during 60 t LD Tapping
Song Shengqiang, Xue Zhengliang, Wang Weixiang, Wang Gongliang, Liu Ruining
Special Steel . 2013, (6): 36 -38 .