Effect of Al-Nb on Structure and Tensile Properties of Alloy GH706 for Rotor of 700 ℃ Power Unit
Bai Yaguan, Nie Yihong, Zhu Huaishen, Zhao Shuai , Yin Fuxing
Special Steel . 2013, (4): 62 -66 .