ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Concasting Parameter and F-EMS on Center Carbon Segregation of 82B Steel Billet
Wang Tao, Chen Weiqing , Wang Hongbing, Wang Jianzhong, Zhang Zhiqiang
Special Steel . 2013, (1): 49 -51 .