Hot Deformation Behavior and Dynamic Recrystallization of Cold Heading Steel SWRCH22A
Ding Bei , Zhao Gang , Ye Chuanlong , Cheng Jian , Yang Lin , Li Zhengsong, Wei Fulong
Special Steel . 2013, (1): 62 -65 .