Effect of Al 2O 3 -SiO 2 -CaO Refining Slag Series on Morphology Control of Inclusions in Spring Steel 55SiCrA
Wang Xianghong, Zhou Li, Liu Tianquan , Meng Yuyong
Special Steel . 2013, (3): 14 -17 .