Effect of Basicity of Tundish Covering Flux on Metallurgy Quality of Ferrite Stainless Steel
Wang Wei , Zhang Runping , Ren Guo , Yang Ruijun, Bai Jingang
Special Steel . 2013, (3): 45 -46 .