Analysis of Commercial Production Test on Metallurgical Functions of an 80 t Single Snorkel Vacuum Refining Furnace
Duan Jianping , Zhang Yongliang, Yang Xuemin, Cheng Guoguang, Zhang Jian
Special Steel . 2012, (1): 26 -29 .