ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Simulation Control Rolling in Laboratory and Quenching-Tempering Treatment on Structure and Properties of Bridge Steel Q690q
Xiong Wenjuan , Yu Chibin , Ye Chuanlong , Xue Gang, Xiao Aida , Yang Hui
Special Steel . 2012, (1): 60 -62 .