Effect of Quenching-Tempering Process on Microstructure and Properties of Micro-Alloying Q960E Steel 70 mm Thickness Plate
Cheng Huimei , Feng Junpeng , Sun Dianqiang , Ge Yangyang , Wang Limi
Special Steel . 2022, (5): 78 -81 .