Effect of Al, Ti, Nb and Mo Content on γ′and η Precipitated Phase in a New Ni-25Cr-20Co Nickel Base Superalloy
Hao Wenhui , Wu Min , Luo Gang , Wang Jue , Xie Xishan
Special Steel . 2013, (2): 1 -3 .