Numerical Simulation and Optimization on Flow of Cooling Water in Oxygen Lance Nozzle for a 50 t Converter
Sun Yuxia , Han Zhijie , Chang Jinbao , Zhang Chaofa , Li Shuangwu , Xuan Zongyu
Special Steel . 2013, (2): 4 -6 .