Experimental Investigation on Effect of RH Refining Slag Series   and Desulfurization Agent on Desulfurization of Pipeline Steel
Jiang Guilian, Tang Haiyan , Cheng Aiming, Li Haishun, Wang Jinhui , Li Jingshe
Special Steel . 2012, (5): 12 -14 .