Increasing Continuous - Continuous Casting Success Rate of Steel 38CrMoAl by Optimizing Deoxidation Process
Zhou Weiji, Bo Yongming, Ji Haifeng, Pan Li, Zhan Dongping
Special Steel . 2012, (5): 40 -42 .