An Analysis on Forming Mechanism of Longitudinal Crack of N08810 Corrosion Resistant Alloy 200 mm Thickness Casting Slab
Ma Jun , Zheng Hongguang, Huang Jian , Guo Liangliang, Ma Tianjun
Special Steel . 2012, (3): 61 -64 .